Widest and Highest-Grade Caesium Intercepts to Date at Vega including 28.0 m at 8.05% Cs2O and 2.2 m at 26.48% Cs2O
Prnewswire·2026-02-03 22:00

MONTREAL, Feb. 3, 2026 /PRNewswire/ - February 4, 2026 – Sydney, Australia Highlights Continue Reading Figure 1: Drill hole result highlights at the CV13 Pegmatite (caesium). (CNW Group/PMET Resources Inc.) Figure 2: Pollucite with late stage lepidolite (purple) and spodumene/pollucite (white) veining displaying classic "tapioca†texture (white blebs) at a depth of ~126 m in drill hole CV25- 948 from the Vega Zone. Core grades 1.9 m at 17.81% Cs2O (125.0 m to 126.9 m) within a wider mineralized interval of 2 ...